Ferolite 'Extra'



Ferolite 'Extra'

-For medium stress conditions.

-For Water, Steam, naturel gas,petorl, saline solution, alkalies ammonia and mildly aggressive media.

Specification Compliance

IS 2712/1998 Grade W/2, O/2
DIN :3754 IT 200
ASTM:F104 F 112650 M6
BS2815-1973 Grade B
JIS:R3453(1985)Type - 2


Properties Applicable for 1.5 mm thick material as per) IS 2712/1998
Density) 1.7-2.2gm/cm3
Tensile Strenght) >12.8 Mpa.
Compressibility) 6-14%
Recovery) >40%
Stress Relaxation) 17.5 Mpa.
Ignition Loss) <28%
FLUID ABSORPTION) ---
Water)
Mass Increase) <10%
In ASTM OIL No.3)
Thickness Increase)
Mass Increase)
In FUEL B)
Thickness Increase)
Mass Increase)
In IRM 903)
Thickness Increase)
Mass Increase)
Sulphuric Acid (96%))
Thickness Increase)
Tensile Strength Decrease)
Nitric Acid (95%))
Thickness Increase)
Tensile Strength Decrease)
Peak Temp oc) 450
max. Operating Pressure Kg/cm2) 85